CML Hybrid Coaxial Multi-Laser Arc Hybrid Additive Manufacturing System (Updated Version)
The Through 6 fully independently controllable laser modules combined with arc heat source, and 6-channel powder and wire
simultaneous feeding, it realizes multiple hybrid technologies including multi-wavelength laser hybridization, laser-arc hybridization, and wire-powder hybridization. It is suitable for frontier research directions of DED technology such as variable component gradient materials, in-situ alloying AM, high-throughput material preparation, and microstructure regulation. At the same time, it can meet the engineering application requirements of DED technology for improving AM material compatibility, AM efficiency, component precision, performance, and complexity.
| Power Version Selection | |||
| Laser Power | 12kW All IR |
8.4kW IR-Blue Hybrid |
4.8kW All-Blue |
| Wavelength | 1080nm |
1080+450nm |
450nm |
| Rated Power | 42kW |
35kW |
27kW |
| Process Specifications | |||
Laser Head |
Approx. 330×430×618mm / ≤25kg
Single module ≤ 1.9 kg
|
Optical System |
6 independently controllable channels
Single spot φ2 mm
|
Control Cabinet |
700×1050×1578mm
≤400kg
|
Applicable Powder Particle Size |
20~300μm |
| Powder Feeding Speed |
0.4~300 g/min (per channel) Max powder channels: 6 |
Applicable Wire Diameter |
φ0.8-2.0 mm Options: 0.8/1.0/1.2/1.6/ 2.0 |
| Spatter Protection | 6 transverse air knives | Wire Feeding Speed |
0.5-22 m/min Max wire switchable: 4 |
| Applicable Materials | Iron-based, nickel-based, titanium alloys,Aluminum alloys, copper alloys, etc. | ||
01 Energy Source — Precisely Controlled Hybrid Energy Field
• Six independently controllable laser modules
The power and on/off status of each of the 6 laser modules can be configured independently, realizing controlled directionally uniform / non-uniform energy distribution. In uniform mode, stable deposition withdirection-independent, low thermal gradient, and low stress is obtained; in non-uniform mode, azimuthal energyshaping is realized, which is key to thermal control at repair boundaries, variable-geometry adaptation, gradedmaterials, and residual stress management.
• Multi-wavelength laser coaxial hybridization
Each of the 6 laser modules can be configured with a different wavelength, expanding the material application range,improving the absorptivity of high-reflectivity metal materials such as copper and aluminum, while remaining
cost-effective.
• 10kW-level high power
Power is upgraded to 12,000 W (All IR)/8,400 W (IR-Blue Hybrid), greatly improving deposition efficiency to meet the
AM needs of high-melting-point materials and large components.
• Laser-Arc hybrid energy field
The coaxial laser and arc hybridization produces a molten pool stirring effect, achieving more complete metallurgical
bonding and a denser microstructure. Alternating the two processes combines the precision of the laser with the efficiency of the arc, simultaneously improving AM efficiency, component performance, and structural complexity.
02 Raw Materials — Free Combination of Multiple Forms and Compositions
• 4-channel wire switching kit, including wire grinder (Optional)
Used together with the grinder, the kit enables rapid switching between multiple wires, improving process flexibility.
• 6 independently controlled powder channels + 1 wire channel for free composition adjustment
Powder channels support up to 6 independent powder material inputs; in-situ alloying can be realized withoutpre-mixing when using multiple materials; free composition adjustment enables frontier research into graded materials and high-entropy alloys.
03 Process Control
• Vision-based adaptive defocus control (Optional)
Real-time visual inspection and adaptive defocus distance adjustment ensure the stability of the AM process.